Differential Scanning Calorimetry (DSC)

DSC is mainly used for analysing plastics, polymer fibers and coatings. Determination of melt temperature (Tm), glass transition temperature (Tg), Oxidation Induction Temperature- or Time (OIT) are very common. OIT is an indirect measure of the ability of a material to resist degradation by oxidation in air. Also curing reaction may be analysed.


This service is also relevant in: Metrology, Construction, Plastics

Service details

Service
Differential Scanning Calorimetry (DSC)
Metrology Area
Gas flow, Temperature
Delivery level
Accredited, Non-accredited
Standards

ISO 11357

Price
Price on tender
Delivery time

Results are delivered within two weeks after samples have arrivet at RISE:s laboratory.  


Order

CAPTCHA
By submitting the form, RISE will process your personal data.

Anna Bondeson

Forsknings- och utvecklingsingenjör
+46 10 516 55 30 Read more about Anna

Contact Anna

CAPTCHA

* Mandatory 

By submitting the form, RISE will process your personal data.

Emelie Palm

Forsknings- och utvecklingsingenjör
+46 10 228 49 57 Read more about Emelie

Contact Emelie

CAPTCHA

* Mandatory 

By submitting the form, RISE will process your personal data.

Purpose

Most polymers have specific melt temperatures, or glass transition temperatures. Therefore DSC is often used to identify plastics and plastic mixtures. For identification of un-known samples DSC-analysis is often  combined with FTIR (Fourier Transform Infrared) Spectroscopy. 

Degree of crystallinity, miscibility of different polymers, curing reactions as well as heat capacity may be analysed. A very common analysis is oxidation stability of polyethylene or polypropylene. A sample is heated in air/oxygen and the time to thermal oxidaton or degradation is measured.

Method

In DSC thermal properties in an material  are measured as a function temperature. A small test sample, typically 5-10 mg is placed in sample holder and heated at a constant rate or is held at constant tempererature. An empty crucible is placed in the instrument oven together with the test sample. Sample and reference are exposed to the same temperature program and the difference in temperature at thermal transitionis is registered. Melting of the sample needs more energy compared to the reference and causes a temperature difference, which is recorded in a thermogram. 

The instrument temperature measure samples from -50°C up to 1100 °C and the heating rate varies between 0,1 till 100°C per minute. 

DSC instruments are found at several locations at RISE and we collaborate to give our clients the best service and delivery time. In Mölndal the core comtenece is recycling and material formulation and processing  in Borås our expertise is focused on polymer constructon materials and accelerated ageing , in Göteborg plastic pipes are analysed and in Stockholm/Kista we have competence on polymers used in chemical process industry.

Deliveries

Test results are delivered in a technical report including thermogram, where method used is described and results are explained.